Publications and Patents

2019

  • Stable Crack Propagation in Free Standing Thermal Sprayed Al2O3 and Al2O3-ZrO2-TiO2 Coat-ings
    M. Neumann, P. Gehre, J. Kübler, N. Dadivanyan, H. Jelitto, G. A. Schneider, C. G. Aneziris:
    Ceramics International 45/7A (2019) 8761–8766, DOILINK

  • YSZ Hollow Sphere Photonic Glasses: Tailoring Optical Properties for Highly Saturated Non-Iridescent Structural Coloration
    Häntsch, Y., Shang, G., Petrov, A., Eich, M., Schneider, G.A.
    Advanced Optical Materials 1900428 (2019). LINK

  • Fracture Toughness of Porous Materials – Experimental Methods and Data
    H. Jelitto, G. A. Schneider:.
    Data in brief 23 (2019) 103709, DOI: LINK

  • Advancing the fabrication of YSZ-inverse photonic glasses for broadband omnidirectional reflector films
    do Rosário, J.J., Häntsch, Y., Pasquarelli, R.M., Dyachenko, P.N., Vriend, E., Petrov, A.Y., Furlan, K.P., Eich, M., Schneider, G.A.
    Journal of the European Ceramic Society 39, 3353-3363 (2019).LINK

  • Highly selective photonic glass filter for saturated blue structural color
    Shang, G., Häntsch, Y., Furlan, K.P., Janßen, R., Schneider, G.A., Petrov, A., Eich, M.
    APL Photonics 4, 046101 (2019). LINK

  • Data Science Based Mg Corrosion Engineering
    Tim Würger, Christian Feiler, Félix Musil, Gregor B. V. Feldbauer, Daniel Höche, Sviatlana V. Lamaka, Mikhail L. Zheludkevich and Robert H. Meißner
    Frontiers in Materials, 6 (2019) 53, Publication Date: 05. April 2019, doi:  10.3389/fmats.2019.00053

  • Hierarchical supercrystalline nanocomposites through the self-assembly of organically-modified ceramic nanoparticles
    Berta Domènech, Michael Kampferbeck, Emanuel Larsson, Tobias Krekeler, Büsra Bor, Diletta Giuntini, Malte Blankenburg, Martin Ritter, Martin Müller, Tobias Vossmeyer, Horst Weller, Gerold A. Schneider
    Nature Scientific Reports (2019) 9:3435

  • Nanoindentation-based study of the mechanical behavior of bulk supercrystalline ceramic-organic nanocomposites
    Büsra Bor, Diletta Giuntini, Berta Domènech, Michale V. Swain, Gerold A. Schneider
    Journal of the European Ceramic Society, xxx (xxxx) xxx

2018

  • Dielectric breakdown toughness from filament induced dielectric breakdown in borosilicate glass
    Pia-Kristina Fischer, Gerold A. Schneider
    J. Eur. Ceram. Soc. 38 (2018) 4476-4482

  • Adsorption of Acetone on Rutile TiO2: A DFT and FTIRS Study
    Tim Würger, Wolfgang Heckel, Kai Sellschopp, Stefan Müller, Andreas Stierle, Yuemin Wang, Heshmat Noei, and Gregor Feldbauer
    J. Phys. Chem. C, 2018, 122 (34), pp 19481–19490, Publication Date (Web): August 20, 2018 (Article)
    DOI: 10.1021/acs.jpcc.8b04222, LINK

  • Suppression of material transfer at contacting surfaces: the effect of adsorbates on Al/TiN and Cu/diamond interfaces from first-principles calculations
    Gregor Feldbauer, Michael Wolloch, Pedro O. Bedolla, Josef Redinger, András Vernes and Peter Mohn
    Journal of Physics: Condensed Matter, 2018, 30 (10), p 105001, DOI: 10.1088/1361-648X/aaac91 LINK

  • The Role of Carbon and Tungsten Disulphide Nanotubes in the Fracture of Polymer-Interlayered Ceramic Composites: a Micro-scopy Study
    K. Livanov, H. Jelitto, G. A. Schneider, H. D. Wagner:.
    J. Mater. Sci. 53/8 (April 2018) 5879–5890, DOILINK

  • Comparative Study of Static and Cyclic Fatigue of ZrB2-SiC Ceramic Composites
    M. Lugovy, N. Orlovskaya, V. Slyunyayev, E. Mitrentsis, M. Neumann, C. G. Aneziris, H. Jelitto, G. A. Schneider, J. Kuebler:.
    J. Eur. Ceram. Soc. 38/4 (April 2018) 1128–1135, DOILINK

  • A Geometric Model for the Fracture Toughness of Porous Materials
    H. Jelitto, G. A. Schneider:.
    Acta Mater. 151 (2018) 443–453, DOILINK

  • R-Curve Behavior and Flexural Strength of Zirconia-toughened Alumina and Partially Stabilized Zirconia Composite Laminates
    D. Blaese, T. Benitez, M. Barros, H. Jelitto, N. Travitzky, D. Hotza, R. Janssen
    Ceramics International 44/12 (2018) 13463–13468, DOILINK

  • Advancing the fabrication of YSZ-inverse photonic glasses for broadband omnidirectional reflector films
    J. J. do Rosário, Y. Häntsch, R. M. Pasquarelli, P. N. Dyachenko, E. Vriend, A. Y. Petrov, K. P. Furlan, M. Eich, G. A. Schneider
    Journal of the European Ceramic Society (2019) DOI: 10.1016/j.jeurceramsoc.2019.04.028

  • Highly selective photonic glass filter for saturated blue structural color
    G. Shang, Y. Häntsch, K. P. Furlan, R. Janßen, G. A. Schneider, A. Petrov, M. Eich
    APL photonics 4/4 (2019) DOI: 10.1063/1.5084138

  • High-temperature stable inverse opal photonic crystals via mullite-sol-gel infiltration of direct photonic crystals
    P. Bueno, K. P. Furlan, D. Hotza, R. Janssen
    Journal of the American Ceramic Society 102/2 (2018) DOI: 10.1111/jace.16012

  • Nanotomography of Inverse Photonic Crystals Using Zernike Phase Contrast
    S. Flenner, E. Larsson, K. Furlan, D. Laipple, M. Storm, F. Wilde, R. Blick, G. A. Schneider, R. Zierold, R. Janssen, others
    Microscopy and Microanalysis 24/S2 (2018), 148–149 DOI: 10.1017/S1431927618013120

  • Dataset of ptychographic X-ray computed tomography of inverse opal photonic crystals produced by atomic layer deposition
    K. P. Furlan, E. Larsson, A. Diaz, M. Holler, T. Krekeler, M. Ritter, A. Y. Petrov, M. Eich, R. Blick, G. A. Schneider, I. Greving, R. Zierold, R. Janßen
    Data in brief 21 (2018), 1924–1936 DOI: 10.1016/j.dib.2018.10.076

  • Photonic materials for high-temperature applications: Synthesis and characterization by X-ray ptychographic tomography
    K. P. Furlan, E. Larsson, A. Diaz, M. Holler, T. Krekeler, M. Ritter, A. Y. Petrov, M. Eich, R. Blick, G. A. Schneider, I. Greving, R. Zierold, R. Janßen
    Applied Materials Today 13 (2018), 359–369 DOI: 10.1016/j.apmt.2018.10.002

  • Self-lubricating composites containing MoS2: A review
    K. P. Furlan, J.D.B. de Mello, A. N. Klein
    Tribology International 120 (2018), 280–298 DOI: 10.1016/j.triboint.2017.12.033

  • On the systematic documentation of the structural characteristics of bovine enamel: A critic to the protein sheath concept
    Ezgi D. Yilmaz, Jasmin Koldehoff, Gerold A. Schneider
    Dental Materials, Volume 34, Issue 10 (October 2018) Pages 1518-1530

  • Hierarchical microcrack model for materials exemplified at enamel
    H. Özcoban, E.D. Yilmaz, G.A. Schneider
    Dental Materials 34 (2018) 69-77

  • Mechanical Behaviour of Zirconia-Toughened Alumina Laminates with or without Y-PSZ Intermediate Layers
    M.D. Barros, P.L. Rachadel, M.C. Fredel, R. Janssen, D. Hotza
    Journal of Ceramic Science and Technology, Vol. 9, No. 1, 69-78

2017

  • Effect of processing route on the microstructure and mechanical properties of hot work tool steel
    R. Besler, M. Bauer, K. P. Furlan, A. N. Klein, R. Janssen
    Materials Research 20/6 (2017), 1518-1524 DOI: 10.1590/1980-5373-MR-2016-0726

  • Microstructural Characterization of Solid State Reaction Phase Formed during Sintering of Hexagonal Boron Nitride with Iron
    K. P. Furlan, D. R. Consoni, B. Leite, M.V.G. Dias, A. N. Klein
    Microscopy and Microanalysis 23/5 (2017), 1061-1066 DOI: 10.1017/S1431927617012478

  • Metallurgical Aspects of Self-lubricating Composites Containing Graphite and MoS2
    K. P. Furlan, P. da Costa Gonçalves, D. R. Consoni, M.V.G. Dias, G. A. de Lima, J.D.B. de Mello, A. N. Klein
    Journal of Materials Engineering and Performance 26/3 (2017), 1135-1145 DOI: 10.1007/s11665-017-2563-4

  • Low-Temperature Mullite Formation in Ternary Oxide Coatings Deposited by ALD for High-Temperature Applications
    K. P. Furlan, T. Krekeler, M. Ritter, R. Blick, G. A. Schneider, K. Nielsch, R. Zierold, R. Janßen  .
    Advanced Materials Interfaces 4/23 (2017) DOI: 10.1002/admi.201700912

  • Highly porous α-Al2O3 ceramics obtained by sintering atomic layer deposited inverse opals
    K. P. Furlan, R. M. Pasquarelli, T. Krekeler, M. Ritter, R. Zierold, K. Nielsch, G. A. Schneider, R. Janssen
    Ceramics international 43/14 (2017), 11260-11264 DOI: 10.1016/j.ceramint.2017.05.176

  • Mechanical Strength and Defect Distribution in Flash Sintered 3YSZ
    J. G. Pereira da Silva, A. N. Yamchelou, A. Debris, C. Wieck, H. Jelitto, H. A. Al-Qureshi, R. Janssen:. J. Eur. Ceram. Soc. 37/8 (July 2017) 2901-2905, DOILink
  • Nanoparticle Growth within Clay – Polymer Nacre-Inspired Materials for Improved Catalysis and Plasmonic Detection in Complex Biofluids
    E. H. Hill, C. Hanske, A. Johnson, L. Yate, H. Jelitto, G. A. Schneider, L. M. Liz-Marzan:
    Metal. Langmuir 33 (2017) 8774–8783, DOILINK

  • How silver segregation stabilizes 1D surface gold oxide: a cluster expansion study combined with ab initio MD simulations
    Hoppe, S., Li, Y., Moskaleva, L.V., Müller, S.
    Physical Chemistry Chemical Physics 19, 14845-14853 (2017). LINK
  • Thermostat Influence on the Structural Development and Material Removal during Abrasion of Nanocrystalline Ferrite
    Eder, S.J.,Cihak-Bayr, U., Bianchi, D., Feldbauer, G., Betz, G.
    ACS Applied Materials & Interfaces 9, 13713-13725 (2017). LINK
  • Oxygen-vacancy driven elctron localization and itinerancy in rutile-based TiO2
    Lechermann, F., Heckel, W., Kristanovski, O., Müller, S.
    Physical Review B, 195159 (2017). LINK
  • Van der Waals Interaction Really Maters: Energetics of Benzoic Acid on TiO2 Rutile Surfaces
    Heckel, W., Würger, T., Müller, S., Feldbauer, G.
    The Journal of Chemistry C, 17207-17214 (2017). LINK
  • A first principles study on the electronic origins of silver segregation at the Ag-Au (111) surface
    Hoppe, S., Müller, S.
    Journal of Applied Physics 122, 235303 (2017). LINK

2016

  • Surface excess elasticity of gold: Ab initio coefficients and impact on the effective elastic response of nanowires
    Elsner, B.A.M., Müller, S., Bargmann, S., Weissmüller, J.
    Acta Materialia 124, 468-477 (2016). LINK
  • Shear Strength and Interfacial Toughness Characterization of Sapphire-Epoxy Interfaces for Nacre-Inspired Composites
    Behr, S., Jungblut, L., Swain, M.V., Schneider, G.A.
    ACS Applied Materials & Interfaces 8, 27322-27331 (2016). LINK
  • Tailoring Toughness and Mechanical Reliability by Contolled Defects: Nature-Inspired Composite Laminates of Laser-Perforated Yttria-Stabilized Zirconia
    Behr, S., Köllner, A., Schneider, G.A.
    Advanced Engineering Materials 18, 1877-1883 (2016). LINK
  • Structure and ordering of oxygen on unreconstructed Ir(100)
    Ferstl, P., Schmitt, T., Schneider, M.A., Hammer, L., Michl, A., Müller, S.
    Physical Review B 93, 235406 (2016). LINK
  • Energy and Spectroscopic Line Shape of the C-O Stretch Mode on Ir(111) in the Presence of Organic Molecules
    Endlich, M., Michl, A., Hildisch, J., Müller, S., Kröger, J.
    The Journal of Physical Chemistry C 120, 11490-11497 (2016). LINK
  • Reaction-forming of ceramic composites using metallic aluminum
    Janssen, R., Travitzky, N., Greil, P., Claussen, N.
    in: Engineered Ceramics: Current Status and Future Prospects, First Edition (2016). LINK
  • Self-assembly of nanoscale lateral segregation profiles
    Stania, R., Heckel, W., Kalichava, I., Bernard, C., Kerscher, T.C., Cun, H.Y., Willmott, P.R., Schönfeld, B., Osterwalder, J., Müller, S., Greber, T.
    Physical Review B 93, 161402(R) (2016). LINK
  • A dynamic bifurcation criterion for thermal runaway during the flash sintering of ceramics
    Pereira da Silva, J.G., Al-Qureshi, H.A., Keil, F., Janssen, R.
    Journal of the European Ceramic Society 36, 1261-1267 (2016). LINK

2015

  • Sintering Simulation of Macro Porous Alumina
    Besler, R., da Silva, Marcel R., do Rosario, J.J., Dosta, M., Heinrich, S., Janssen, R.
    Journal of the American Ceramic Society 98, 3496-3502 (2015). LINK
  • How the aggregation of oxygen vacancies in rutile-based TiO2-δ phases causes memristive behavior
    Heckel, W., Wehlau, M., Maisel, S.B., Frauenheim, T., Knaup, J.M., Müller, S.
    Physical Review B 92, 214104 (2015). LINK
  • High Temperature Behavior of Monodisperse Porosity in Alumina Films
    Pasquarelli, R.M., do Rosario, J.J., Rath, L., Schneider, G.A., Janssen, R.
    Journal of the European Ceramic Society 35, 3917-3926 (2015). LINK
  • Synthesis and Thermal Stability of ZrO2 and YSZ Microspheres
    Leib, E.W., Vainio, U., Pasquarelli, R.M., Kus, J., Czaschke, C., Walter, N., Janssen, R., Müller, M., Schreyer, A., Weller, H., Vossmeyer, T.
    Journal of Colloid and Interface Science 44, 582-592 (2015). LINK
  • Temperature Distributions during the Flash Sintering of 8% Yttria-Stabilized Zirconia
    Pereira da Silva, J.G., Lebrun, J.-M., Al-Qureshi, H.A., Janssen, R., Raj, R.
    Journal of the American Ceramic Society 98, 3525-3528 (2015). LINK
  • Processing of All-Oxide Ceramic Matrix Composites with RBAO Matrix
    Guglielmi, P.O., Garcia, D.G., Hablitzel, M.P., Blaese, D., Goulart, D., Borchert, A., Hotza, D., Janssen, R.
    Journal of Ceramic Science and Technology, in print (2015).
  • Enhanced Structural and Phase Stability of Titania Inverse Opals
    Pasquarelli, R.M., Lee, H.S., Kubrin, R., Zierold, R., Petrov, A.Y., Nielsch, K., Schneider, G.S., Janssen, R.
    Journal of the European Ceramic Society 35, 3103-3109 (2015). LINK
  • Mechanical tests and simulations on load sharing in alumina fiber bundles
    Neckel, L., Pereira da Silva, J.G., Guglielmi, P., Hotza, D., Al-Qureshi, H.A., Monteldo, O.R.K., Bergmann, C.P., Janssen, R.
    Ceramics International 41, 13257-13263 (2015). LINK
  • Surface Morphology and Fracture Strength Analysis of Nanosecond Ablated Alumina
    Gomez, D.R., Hallmann, S., Daniel, C., Fredel, M.C., Janssen, R.
    Journal of Ceramic Society of Japan 123, 160-166 (2015). LINK
  • Size effects and strain localization in atomic-scale cleavage modeling
    Elsner, B.A.M., Müller, S.
    Journal of Physics: Condensed Matter 27, 345002 (2015). LINK
  • Solubility and ordering of Ti, Ta, Mo and W on the Al sublattice in Li2-Co3Al
    Koßmann, J., Hammerschmidt, T., Maisel, S., Müller, S., Drautz, R.
    Intermetallics 64, 44-50 (2015). LINK
  • Large-scale parallel alignment of platelet-shaped particles through gravitational sedimentation
    Behr, S., Vainio, U., Müller, M., Schreyer, A., Schneider, G.A.
    Scientific Reports 5, 9984 (2015). LINK
  • Electrical conduction mechanism in bulk ceramic insulators at high voltages until dielectric breakdown
    Neusel, C., Jelitto, H., Schneider, G.A.
    Journal of Applied Physics 117, 154902 (2015). LINK
  • ZrO2 fiber-matrix interfaces in alumina fiber-reinforced model composites
    Blaese, D., Garcia, D.E., Guglielmi, P.O., Hotza, D., Fredel, M.C., Janssen, R.
    Journal of the European Ceramic Society 35, 1593-1598 (2015). LINK
  • Microstructure and flexural properties of multilayered fiber-reinforced oxide composites fabricated by a novel lamination route
    Guglielmi, P.O., Blaese, D., Hablitzel, M.P., Nunes, G.F., Lauth, V.R., Hotza, D., Al-Qureshi, H.A., Janssen, R.
    Ceramics International 41, 7836-7846 (2015). LINK
  • Highly-Structured, Additive-Free Lithium-Ion Cathodes by Freeze-Casting Technology
    Behr, S., Amin, R., Chiang, Y.-M., Tomsia, A.P.
    Ceramic Forum International 92, vol. 4, 39-43 (2015).
  • Self-Assembled Ultra High Strength, Ultra Stiff Mechanical Metamaterials Based on Inverse Opals
    do Rosário, J.J., Lilleodden, E.T., Waleczek, M., Kubrin, R., Petrov, A.Y., Dyachenko, P.N., Sabisch, J.E.C., Nielsch, K., Huber, N., Eich, M., Schneider, G.A.
    Advanced Engineering Materials (2015). LINK
  • Thickness-dependence of the breakdown strength: Analysis of the dielectric and mechanical failure
    Neusel, C., Jelitto, H., Schmidt, D., Janssen, R., Felten, F., Schneider, G.A.
    Journal of the European Ceramic Society 35, 113-123 (2015). LINK
  • Transparent nanophosphor films with high quantum efficiency through cold compaction
    Kubrin, R., do Rosário, J.J., Schneider, G.A.
    RSC Advances 5, 25555-25564 (2015). LINK
  • Influence of structural hierarchy on the fracture behavior of tooth enamel
    Yilmaz, E.D., Schneider, G.A., Swain, M.V.
    Philosophical Transactions A 373 (2015). LINK
  • Uniaxial compressive behavior of micro-pillars of dental enamel characterized in multiple directions
    Yilmaz, E.D., Jelitto, H., Schneider, G.A.
    Acta Biomaterialia (2015). LINK
  • Damage modelingof small-scale experiments on dental enamel with hierarchical microstructure
    Scheider, I., Xiao, T., Yilmaz, E., Schneider, G.A., Huber, N., Bargmann, S.
    Acta Biomaterialia (2015). LINK

2014

  • Nickel-rhenium compound sheds light on the potency of rhenium as a strengthener in high-temperature nickel alloys
    Maisel, S., Schindzielorz, N., Mottura, A., Reed, R.C., Müller, S.
    Physical Review B 90, 094110 (2014). LINK
  • Multilayered Fiber-Reinforced Oxide Composites Produced by Lamination of Thermoplastic Prepregs
    Guglielmi, P.O., Blaese, D., Hablitzel, M., Nunes, G., Lauth, V.R., Garcia, D., Al-Qureshi, H.A., Hotza, D., Janssen, R.
    Advances in Science and Technology 89, 145-150 (2014). LINK
  • Characterization of Young Modulus and Fracture Toughness of Albite Glass by Different Techniques
    Sousa, F., Dal Bó, M., Guglielmi, P.O., Janssen, R., Hotza, D.
    Ceramics International 40, 10893-10899 (2014). LINK
  • Discovery of a thermally persistent h.c.p. solid-solution phase in the Ni-W system
    Kurz, S.J.B., Maisel, S., Leineweber, A., Höfler, M., Müller, S., Mittemeijer, E.J.
    Journal of Applied Physics 116, 083515 (2014). LINK
  • Micromechanical characterization of prismless enamel in the tuatara, Sphenodon punctatus
    Yilmaz, E.D., Bechtle, S., Özcoban, H., Kieser, J.A., Swain, M.V., Schneider, G.A.
    Journal of the Mechanical Behavior of Biomedical Materials 39, 210-217 (2014). LINK
  • Ab-initio modeling of electromechanical coupling at Si surfaces
    Hoppe, S., Michl, A., Weissmüller, J., Müller, S.
    Journal of Applied Physics 116, 073507 (2014). LINK
  • Facile Deposition of YSZ-Inverse Photonic Glass Films
    do Rosario, J.J., Dyachenko, P.N., Kubrin, R., Pasquarelli, R.M., Petrov, A.Y., Eich, M., Schneider, G.A.
    ACS Applied Materials & Interfaces 6, 12335-12345 (2014). LINK
  • Phase behavior and mechanical properties of Ni-W studied by first-principles calculations and ab initio based thermodynamics
    Schindzielorz, N., Nowak, K., Maisel, S. B., Müller, S.
    Acta Materialia 75, 307-315 (2014). LINK
  • The Role of Hydrogen on the Adsorption Behavior of Carboxylic Acid on TiO2 Surfaces
    Heckel, W., Elsner, B.A.M., Schulz, C., Müller, S.
    Journal of Physical Chemistry C 118, 10771-10779 (2014). LINK

 

2013

  • Towards bio-inspired engineering materials: Modeling and simulation of the mechanical behavior of hierarchical bovine dental structure
    Bargmann, S., Scheider, I., Xiao, T., Yilmaz, E., Schneider, G.A., Huber, N.
    Computational Materials Science 79, 390-401 (2013). LINK
  • Surface Properties of Alloys
    Kerscher, T. C., Müller, S., in Surface and Interface Science, Volume 3 (2013), Klaus Wandelt, pp. 1-59, LINK
  • Fracture toughness and corrosion behaviour of infiltrated Al2O3|P - Steel composites
    Schlenther, E., Özcoban, H., Jelitto, H., Faller, M., Schneider, G.A., Graule, T., Aneziris, C.G., Kuebler, J.
    Materials Science and Engineering: A 590, 132-139 (2013). LINK
  • Biomechanical adaptation of the bone-periodontal ligament (PDL)-tooth fibrous joint as a consequence of disease
    Lin, J.D., Lee, J., Özcoban, H., Schneider, G.A., Ho, S.P.
    Journal of Biomechanics (2013). LINK
  • Dependence of the breakdown strength on thickness and permittivity
    Neusel, C., Schneider, G.A.
    2013 IEEE International Conference on Solid Dielectrics, Bologna, Italy, 31-35 (2013). LINK
  • Size-dependence of the dielectric breakdown strength from nano- to millimeter scale
    Neusel, C., Schneider, G.A.
    Journal of the Mechanics and Physics of Solids (2013). LINK
  • Sign-inverted response of aluminum work function to tangential strain
    Michl, A., Weissmüller, J., Müller, S.
    Journal of Physics: Condensed Matter 25, 445012 (2013). LINK
  • Structure and electrical properties of 0.85(Bi0.5Na0.5)TiO3-0.12BaTiO3-0.03SrTiO3 ferroelectric ceramics
    Mgbemere, H.E., Fernandes, R.P., Schneider, G.A.
    Journal of the European Ceramic Society 33, 3015-3022 (2013). LINK
  • A novel method for a multi-level hierarchical composite with a brick-and-mortar structure
    Brandt, K., Wolff, M.F.H., Salikov, V., Heinrich, S., Schneider, G.A.
    Scientific Reports 3, 2322 (2013). LINK
  • An accidental visualization of the Brillouin zone in an Ni-W alloy via diffuse scattering
    Maisel, S.B., Schindzielorz, N., Müller, S., Reichert, H., Bosak, A.
    Journal of Applied Crystallography 46, 1211-1215 (2013). LINK
  • Dielectric behaviour and conductivity of high-filled BaTiO3-PMMA-composites and the facil route of emulsion polymerization in synthesizing the same
    Brandt, K., Neusel, C., Behr, S., Schneider, G.A.
    Journal of Materials Chemistry C 1, 3129-3137 (2013). LINK
  • A giffith type energy release rate model for dielectric breakdown under space charge limited conductivity
    Schneider, G.A.
    Journal of the Mechanics and Physics of Solids 61, 78-90 (2013). LINK
  • Interfaces in metamict titanite: the macroscopic mechanical properties after stepwise annealing
    Beirau, T., Guglielmi, P., Paulmann, C., Schneider, G.A., Groat, L.A., Malcherek, T., Salje, E.K.H, Bismayer, U.
    Phase Transitions: A Multinational Journal 86 (1) (2013). LINK
  • Biomechanics of a bone-peridontal ligament-tooth fibreous joint
    Lin, J.D., Özcoban, H., Greene, J.P., Jang, A.T., Djomehri, S.I., Fahey, K.P., Hunter, L.L., Schneider, G.A., Ho, S.P.
    Journal of Biomechanics 46 (3), 443-449 (2013). LINK

 

 

2012  

  • Adsorbate-induced segregation: First-principles study for C/Pt25Rh75(100)
    Kerscher, T.C., Landgraf, W., Podloucky, R., Müller, S.
    Physical Review B 86 (19) 195420 (2012). LINK
  • A canonical stability-elasticity relationship verified for one million face-centered-cubic structures
    Maisel, S.B., Höfler, M., Müller, S.
    Nature 491, 740-743 doi: 10.1038/nature11609 (2012). LINK
  • Stacking of Ceramic Inverse Opals with Different Lattice Constants
    Kubrin, R., Lee, H.S., Zierold, R., Petrov, A. Y., Janssen, R., Nielsch, K., Eich, M., Schneider, G.A.
    Journal of the American Ceramic Society 95 (7), 2226-2235 (2012). LINK
  • Mechanical characterization of highly porous β-Si3N4 ceramics fabricated via partial sintering & starch addition
    Kalemtas, A., Topates, G., Özcoban, H., Mandal, H., Kara, F., Janssen R.
    Journal European Ceramic Society, DOI: 10.1016/j.jeurceramsoc.2012.10.036 (2012). LINK
  • Solutions for Impact over Aerospace Protection
    Neckel, L., Hotza, D., Stainer, D., Janssen, R., Lezana, A.G.R., Dias, A., Al-Qureshi, H.A.
    Key Engineering Materials 488-489, 25-28 (2012). LINK
  • Production of oxide ceramic matrix composites by a prepreg technique
    Guglielmi, P. O., Nunes, G.F., Hablitzel, M. P., Hotza, D., Janssen, R.
    Materials Science Forum 727-728, 556-561 (2012). LINK
  • RBMAO: A novel route for porous matrix composites
    Berti, L.F., Rambo, C.R, Bazzo, E., Janssen, R., Hotza, D.
    Materials Science Forum 727-728, 568-573 (2012). LINK
  • Fiber-matrix compatibility in LZSA glass-ceramic matrix composites
    Goushegir, S. M., Guglielmi, P. O., Oliveira, A.P.N., Hotza, D., Janssen, R.
    Materials Science Forum 727-728, 562-567 (2012). LINK
  • Modeling of ceramic oxide fiber bundles mechanical properties
    da Silva, J.G.P., Hotza, D., Janssen, R., Al-Qureshi, H. A.
    Materials Science Forum 727-728, 574-580 (2012). LINK
  • Interaction of cartilage and ceramic matrix
    Wiegandt, K., Goepfert, C., Pörtner, R., Janssen, R.
    Tissue Engineering III: Cell - Surface Interactions for Tissue Culture, Series: Advances in Biochemical Engineering Biotechnology, Springer-Verlag, Berlin-Heidelberg 126, 297-315 (2012). LINK
  • Ultrasonic characterization of defective porcelain tiles
    Eren, E., Kurama, S., Janssen, R.
    Boletin de Sociedad Espanola de Ceramica y Vdrio, 51 (4), 211-216 (2012). LINK
  • Fracture behavior of hydroxyapatite nanofibers in dental enamel under micro-pillar compression
    Yilmaz, E.D.; Bechtle, S.; Özcoban, H.; Schreyer, A.; Schneider, G.A.
    Scripta Materialia doi: org/10.1016/j.scriptamat.2012.11.007 (2012). LINK
  • Structural phase transitions and electrical properties of (KxNa1-x)NbO3-based ceramics modified with Mn
    Mgbemere, H.E.; Hinterstein, M.; Schneider, G.A.
    Journal of the European Ceramic Society 32, 4341-4352 (2012). LINK
  • First-principles study of hydrogen ordering in lanthanum hydride and its effect on the metal-insulator transition
    Kerscher, T.C.; Schöllhammer, G.; Herzig, P.; Wolf, W.; Podloucky, R.; Müller, S.
    Physical Review B 86 014107 (2012). LINK
  • First-principles modeling of temperature- and concentration-dependent solubility in the phase-separating alloy FexCu1-x
    Reith, D.; Stöhr, M.; Podloucky, R.; Kerscher, T.C.; Müller, S. 
    Physical Review B 86, 020201(R) (2012). LINK
  • Automated control of stable crack growth for r-curve measurements in brittle materials
    Jelitto H.; Hackbarth, F.; Özcoban, H.; Schneider, G.A.
    Experimental Mechanics doi: 10.1007/s11340-012-9622-4 (2012). LINK
  • Investigation of fracture toughness of modified (KxNa1-x)NbO3 lead-free piezoelectric ceramics
    Yilmaz, E.D.; Mgbemere, H.E.; Özcoban, H.; Fernandes, R.P.; Schneider, G.A.
    Journal of the European Ceramic Society 32 (12), 3339-3344 (2012). LINK
  • Thermal radiation transmission and reflection properties of ceramic 3D photovoltaic crystals
    Lee, H.S.; Kubrin, R.; Zierold, R.; Petrov, A.Yu; Nielsch, K.; Schneider, G.A.;  Eich, M.
    Journal of the Optical Society of America B 29, 450-457 (2012). LINK
  • Computer-controlled stable crack growth as a reliable and fast method to determine subcritical crack growth
    Özcoban, H.; Fett, T.; Schneider, G.A.
    Journal of Testing and Evaluation 40 (2), 238-242 (2012). LINK PDF
  • Comparison of mechanical behaviors of inter- and intrarod regions in enamel
    Ang, S.F.; Saadatmand, M.; Swain, M.V.; Klocke, A.; Schneider, G.A.
    Journal of Materials Research 27 (2), 448-456 (2012). LINK
  • No miscibility gap in Pt-Rh binary alloys: A first principles study
    Maisel, S.B.; Kerscher, T.C.; Müller, S.
    Acta Materialia 60 (3), 1093-1098 (2012). LINK
  • Experimental crack front investigation of unpoled soft lead zirconate titanate (PZT) using the single edge V-notched beam (SEVNB) method
    Özcoban, H.; Salikov, V.; Jelitto, H.; Schneider, G.A.
    Experimental Mechanics 52 (9), 1565-1568 (2012). LINK
  • Dielectric breakdown of alumina single crystals
    Neusel, C.; Jelitto, H.; Schmidt, D.; Janssen, R.; Felten, F.; Schneider, G.A.
    Journal of the European Ceramic Society 32 (5), 1053-1057 (2012). LINK 
  • Fiber-Matrix Compatibility in an All-Oxide Ceramic Composite with RBAO Matrix
    Goushegir, S.M.; Guglielmi, P.O.; da Silva, J.G.; Hablitzel, M.P.; Hotza, D.; Al-Qureshi, H.A.; Janssen, R.
    Journal of the American Ceramic Society 95, 159-164 (2011). LINK

  • A method to determine site-specific, anisotropic fracture toughness in biological materials
    Bechtle, S.; Özcoban, H.; Yilmaz, E.D.; Fett, T.; Rizzi, G.; Lilleodden, E.T.; Huber, N.; Schreyer, A.; Swain, M.V.; Schneider, G.A.
    Scripta Materialia 66 (8), 515-518 (2012). LINK 
  •  

2011

  • Towards ceramic 3DOM-materials as novel high-temperature reflective coatings and filters for thermophotovoltaics
    Kubrin, R.; Lee, H.S.; Petrov, A.; Janssen, R.; Schneider, G.A.; Bachmann, J.; Nielsch, K.; Eich, M.
    IOP Conference Series: Materials Science and Engineering 18, 182004 (2011). LINK
  • Deutscher Patentantrag: "Verfahren zur Herstellung eines Verbundwerkstoffs, der Verbundwerkstoff und die Verwendung des Verbundwerkstoffs zur Herstellung bestimmter Produkte"
    Erfinder: Schneider, G.A.; Heinrich, S.; Wolff, M.; Antonyuk, S.; Salikov, V.; Brandt, K.
    Deklarant: Technische Universität Hamburg-Harburg, Aktenzeichen 10 2011 119 939.3, eingereicht am 01.12.2011.
  • Novel ceramic-polymer composites synthesized by compaction of polymer-encapsulated TiO2-nanoparticles
    Brandt, K; Salikov, V.; Özcoban, H.; Staron, P.; Schreyer, A.; Prado, L.A.S.A.; Schulte, K.; Heinrich, S.; Schneider, G.A.
    Composites Science and Technology 72, 65-71 (2011). LINK
  • Hierarchical flexural strength of enamel: transition from brittle to damage-tolerant behaviour
    Bechtle, S.; Özcoban, H.; Lilleodden, E.T; Huber, N.; Schreyer, A.; Swain, M.V.; Schneider, G.A.
    Journal of the Royal Society Interface doi: 10.1098/rsif.2011.0498 (2011). LINK
  • Electrical and structural characterization of (KxNa1-x)NbO3 ceramics modified with Li and Ta
    Mgbemere, H. E.; Hinterstein, M.; Schneider, G. A.
    Applied Crystallography 44, 1080-1089 (2011). LINK
  • Large-scale lattice gas monte carlo simulations for the generalized ising model
    Kerscher, T.C.; Müller, S; Snell, Q.O; Hart, G.L.W.
    2011 IEEE International Parallel & Distributed Processing Symposium, 1234-1241 (2011). LINK
  • Mechanisms of toughening in silicon nitrides: The roles of crack bridging and microstructure
    Fünfschilling, S.; Fett, T.; Hoffmann, M.J.; Oberacker, R.; Schwind, T., Wippler, J.; Böhlke, T.; Özcoban, H.; Schneider, G.A.; Becher, P.F.; Kruzic, J.J.
    Acta Materialia, 59(10), 3978-3989 (2011). LINK
  • Temperature-dependent synchrotron powder diffraction phase strudies of (K0.37Na0.52Li0.03)(Nb0.87Ta0.1Sb0.03)O3 ferroelectric ceramics
    Mgbemere, H. E.; Fernandes, R. P.; Hinterstein, M.; Schneider, G. A.
    Zeitschrift für Kristallographie 226(2), 138-144 (2011). LINK
  • Sub-10-micrometer Toughening and Crack-tip Toughness of Dental Enamel
    Ang, S. F.; Schulz, A.; Pacher Fernandes, R.; Schneider, G. A.
    Journal of the Mechanical Behavior of Biomedical Materials, 4, 423-432 (2011). LINK PDF
  • Influence of small cyclic and DC electrical loads on the fracture toughnesss of ferroelectric ceramics
    Engert, A. R.; Neumeister, P.; Mecklenburg, M; Jelitto, H.; Balke, H.; Schneider, G. A.
    Journal of the European Ceramic Society, 31(4) 531-540 (2011). LINK PDF

 

 

2010

  • Osteoclastic Bioresorption of Biomaterials: Two- and Three- dimensional Imaging and Quantification
    Winkler, T.; Hoenig, E.; Huber, G.; Janssen, R.; Fritsch, D.; Gildenhaar, R.; Berger, G.; Morlock, M. M.; Schilling, A. F.
    Int. J. of Artifical Organs, 33(4), 198-203 (2010). LINK
  • Porous Ceramic Structure for Capillary Pumped Loops
    Berti, L. F.; Santos, P.; Bazzo, E.; Janssen, R.; Hotza, D.; Rambo, C-.R.
    in Current Issues in Organic Chemistry, eds by K. Hadiijanov, V. Valtchev, S. Mintova, G. Vayssilov, Heron Press, Sofia (2010).
  • Volumetric Analysis of Osteolclastic Bioresprotion of Biomaterials with Different Solubility
    Winkler, T.; Hoenig, E.; Gildenhaar, R.; Berger, G.; Fritsch, D.; Janssen, R.; Morlock, M. M. R.; Schilling, A. F.
    Acta Biomaterialia 6(10), 4127-4135 (2010). LINK
  • A Prepreg Approach for Low Cost Oxide-oxide Composites
    Guglielmi, P. O.; Nunes, G. F.; Hotza, D.; Janssen, R.
    in High Temperature Ceramic Materials and Composites, ed. by W. Krenkel, J. Lamon, Aviso, 420 427 (2010).
  • Reaction Formed Alumina-Alumina FRCMC
    Janssen, R.
    in High Temperature Ceramic Materials and Composites, ed. by W. Krenkel, J. Lamon, Aviso, 398- 403 (2010).
  • 3D Bioreactor Cultivation of the Human Hepatoma Cell Line HEPG 2 as a Promising Tool for In Vitro Substance Testing
    Goepfert, C.; Scheurer, W.;Rohn, S.;Rathjen, B.; Meyer, S.; Dittmann, A.; Wiegandt, K.; Janssen, R.; Poertner, R.
    Int. J. of Artifical Organs, 33(7) 440-440 (2010). LINK
  • What do we know about surface charges on cracks in ferroelectric ceramics?
    Engert, A. R.; Felten, F.; Jelitto, H.; Schneider, G. A.
    Proceedings of the IUTAM Symposium on Multiscale Modelling of Fatigue, Damage and Fracture in Smart Materials, Vol. 24, 9-20 (2010). LINK 
  • Determination of the multiaxial failure criteria for alumina ceramics under tension-torsion test
    Nohut, S.; Usbeck, A.; Özcoban, H.; Krause, D.; Schneider, G. A.
    Journal of the European Ceramic Society, 30, 3339-3349 (2010). LINK PDF
  • Predicting the segregation profile of the Pt25Rh75(100) surface from first-principles
    Welker, P.; Wieckhorst, O.; Kerscher, T. C.; Müller, S.
    J. Phys.: Condens. Matter., 22, 384203 (2010). LINK
  • Area fraction quantification of ferroelectric domain orientations in BaTiO3 using piezoresponse force microscopy
    Fernandes, R. P.; Herber, R.-P.; Kunz, L.; Mgbemere, H. E.; Schneider, G. A.
    J. Appl. Phys., 108, 044103 (2010). LINK PDF
    Copyright (2010) American Institute of Physics. This article may be downloaded for personal use only. Any other use requires prior permission of the author and the American Institute of Physics.
  • Effect of antimony substitution for niobium on the crystal structure, piezoelectric and dielectric properties of (K0.5Na0.5)NbOceramics
    Mgbemere, H. E.; Schneider, G. A; Stegk, T. A.
    Functional Materials Letters, 3(1), 25-30 (2010). LINK PDF
    Electronic version of an article published as Functional Materials Letters, 3, 1, 2010, 25-30 [DOI No: 10.1142/S1793604710000841]
  • R curves from compliance and optical crack-length measurements
    Fünfschilling, S.; Fett, T.; Oberacker, R.; Hoffmann, M. J.; Özcoban, H.; Jelitto, H.; Schneider, G. A.; Kruzic, J. J.
    J. Am. Ceram. Soc., 93(9), 2814-2821 (2010). LINK
  • Estimation of the high-hemperature R curve for ceramics from strength measurements including specimens with focused ion beam notches
    Fünfschilling, S.; Fett, T.; Hoffmann, M. J.; Oberacker, R.; Özcoban, H.; Schneider, G. A.; Brenner, P.; Gerthsen, D.; Danzer, R.
    J. Am. Ceram. Soc., 93(9), 2411-2414 (2010). LINK
  • Leading opinion: On the mechanical properties of hierarchically structured biological materials
    Bechtle, S.; Ang, S. F.; Schneider, G. A.
    Biomaterials, 31(25), 6378-6385 (2010). LINK PDF
  • Influence of finite notch root radius and optically determined crack length on the measured fracture toughness of brittle materials
    Özcoban, H.; Jelitto, H.; Schneider, G. A.
    Journal of the European Ceramic Society, 30(7), 1579-1583 (2010). LINK PDF
  • Mixed-mode stress intensity factors for kink cracks with finite kink length loaded in tension and bending: Application to dentin and enamel
    Bechtle, S.; Fett, T.; Rizzi, G.; Habelitz, S.; Schneider, G. A.
    Journal of the Mechanical Behavior of Biomedical Materials, 3, 303-312 (2010). LINK PDF
  • Size-dependent elastic/inelastic behavior of enamel over millimeter and nanometer length scales
    Ang, S. F.; Bortel, E. L.; Swain, M. V.; Klocke, A.; Schneider, G. A.;
    Biomaterials, 31(7), 1955-1963 (2010). LINK PDF
  • The fracture behaviour of dental enamel
    Bechtle, S.; Habelitz, S.; Klocke, A.; Fett, T.; Schneider, G.A.
    Biomaterials, 31(2), 375-384 (2010). LINK PDF
  • Crack arrest within teeth at the dentinoenamel junction caused by elastic modulus mismatch
    Bechtle, S.; Fett, T.; Rizzi, G.; Habelitz, S.; Klocke, A.; Schneider, G. A.;
    Biomaterials, 31, 4238-4247 (2010). LINK PDF

 

2009

  • Determination of the elastic/plastic transition of human enamel by nanoindentation
    Ang, S. F.; Scholz, T.; Klocke, A.; Schneider, G. A.
    Dental Materials, 25(11), 1403-1410 (2009). LINK PDF
  • Investigation of the dielectric and piezoelectric properties of potassium sodium niobate ceramics close to the phase boundary at (K0.35Na0.65)NbO3 and partial substitutions with lithium and antimony
    Mgbemere, H. E.; Herber, R.; Schneider, G. A.
    Journal of the European Ceramic Society, 29(15), 3273-3278 (2009). LINK PDF
  • Effect of MnO2 on the dielectric and piezoelectric properties of alkaline niobate based lead free piezoelectric ceramics
    Mgbemere, H. E.; Herber, R.; Schneider, G. A.
    Journal of the European Ceramic Society, 29(9), 1729-1733 (2009). LINK PDF
  • Elastic to elastic-plastic transition of Al2O3/TiC ceramics studied by nanoindentation
    Zimmermann, K.; Schneider, G. A.
    Journal of Materials Research, 24(6), 1960-1966 (2009). LINK
  • Investigation of phase boundaries in the system (KxNa1-x)1-yLiy(Nb1-zTaz)O3 using high-throughput experimentation (HTE)
    Stegk, T. A.; Mgbemere, H.; Herber, R.; Janssen, R.; Schneider, G. A.
    Journal of the European Ceramic Society, 29(9), 1721-1727 (2009). LINK PDF 
  • Failure probability of ceramic coil springs
    Nohut, S.; Schneider, G. A.
    Journal of the European Ceramic Society, 29(6), 1013-1019 (2009). LINK PDF
  • Chapter "Technical Strategies to Improve Tissue Engineering of Cartilage-Carrier-Constructs" 
    Pörtner, R.; Goepfert, C.; Wiegandt, K.; Janssen, R.; Ilinich, E.; Paetzold, H.; Eisenbarth, E.; Morlock, M.
    in book "Bioreactor Systems for Tissue Engineering", 112, 145-181 (2009). 
  • Bridging stresses from R-curves of silicon nitrides
    Fünfschilling, S.; Fett, T.; Hoffmann, M.; Oberacker, R.; Jelitto, H.; Schneider, G.; Härtelt, M.; Riesch-Oppermann, H.
    Journal of Materials Science, 44(14), 3900-3904 (2009).  PDF
  • Determination of the crack-tip toughness in silicon nitride ceramics
    Fünfschilling, S.; Fett, T.; Hoffmann, M.; Oberacker, R.; Jelitto, H.; Schneider, G.
    Journal of Materials Science, 44(1), 335-338 (2009).  PDF
  • Invention registration at the TUHH: "Automatisierte R-Kurven-Messung"
    Inventors: Jelitto, H.; Hackbarth, F.; Schneider, G. A.
    Internal file number TU 114, September 9th 2009.
  • German patent application (in preparation): "Verfahren und Vorrichtung zur Bestimmung von Riß-Widerstandskurven"
    Inventors: Jelitto, H.; Hackbarth, F.; Schneider, G. A.
    Declarant: Hamburg University of Technology and TuTech Innovation GmbH, (corresponding to internal file number TU 114).
  • Ferroelectric properties of ruthenium-doped lead zinc niobate-lead titanate single crystal
    Scholz, T.; Mihailova, B.; Schneider, G. A.; Pagels, N.; Heck, J.; Malcherek, T.; Fernandes, R. P.; Marinova, V.; Gospodinov, M.; Bismayer, U.
    Journal of Applied Physics, 106, 074108 (2009). LINK
  • Modification of biomaterial surface structure for the in vitro generation of osteochondral implants
    Goepfert, C.; Fritsch, D.; Richter, T.; Janssen, R.; Poertner, R.
    Tissue engineering Part A, BioStar 2008-Science in Exchange Meeting Abstracts. 15(3), 726-727 (2009).

 

2008 

  • Fracture resistance evaluation of RuO2-based thick film resistor material by in situ crack extension observation in a scanning electron microscope
    Dorsch, N. S.; Peshekhodov, I.; Spies, P.; Schneider, G. A.
    Acta Materialia, 56(18), 5027-5033 (2008). LINK
  • Tailor-made ceramic-based components--Advantages by reactive processing and advanced shaping techniques
    Janssen, R.; Scheppokat, S.; Claussen, N.
    Journal of the European Ceramic Society, 28(7), 1369-1379 (2008). LINK
  • Rosette screw arms created by ac-domain structures and dislocations in barium titanate during nanoindentation
    Schneider, G. A.; Scholz, T.; Espinoza-Beltran, F. J.
    Applied Physics Letters, 92(2), 022906-3 (2008). LINK
  • Indentation size effect in soft PZT ceramics with tetragonal structure close to the MPB
    Hurtado-Macias, A.; Munoz-Saldana, J.; Espinoza-Beltran, F. J.; Scholz, T.; Swain, M. V.; Schneider, G. A.
    Journal of Physics D: Applied Physics, 41(3), 035407 (2008). LINK
  • Fracture criterion for a conducting crack in poled PZT-PIC 151 investigated by stable crack growth
    Gehrig, F.; Jelitto, H.; Schneider, G. A.
    Acta Materialia, 56(2), 222-229, (2008). LINK
  • High throughput screening of piezoelectric response of ferroelectric thin films with automated scanning probe microscopy
    Herber, Ralf-Peter; Schröter, Christian; Wessler, Berit; Schneider, Gerold A.
    Thin Solid Films, 516(23), 8609-8612, (2008). LINK
  • R-curve determination for the initial stage of crack extension in Si3N4
    Fett, T.; Fünfschilling, S.; Hoffmann, M. J.; Oberacker, R.; Jelitto, H.; Schneider, G. A.
    Journal of the American Ceramic Society, 91(11), 3638-3642 (2008). LINK
  • Influence of surface modification on the cutting performance of reaction-sintered Al2O3-TiOC Ceramics
    Bhattacharya, A. K.; Zimmermann, K.; Schneider, G. A.; Hintze, W.
    Journal of the American Ceramic Society, 91(9), 2982-2986 (2008). LINK
  • High-Throughput synthesis and characterization of bulk ceramics from dry powders
    Stegk, T. A.; Janssen, R.; Schneider, G. A.
    Journal of Combinatorial Chemistry, 10(2), 274-279 (2008). LINK
  • Viscous flow model of creep in enamel
    Schneider, G. A.; He, Li Hong; Swain, M. V.
    Journal of Applied Physics, 103, 014701 (2008). LINK
  • Estimation of R-curve in WC/Co cermet by CT test
    Felten, F.; Schneider, G. A.; Sadowski, T.
    International Journal of Refractory Metals and Hard Materials, 26(1), 55-60 (2008). LINK
  • In Vitro generation of cartilage-carrier-constructs on hydroxylapatite ceramics with different surface structures
    Wiegandt, K.; Goepfert, C.; Richter, T.; Fritsch, D.; Janssen, R.; Portner, R.
    The Open Biomedical Engineering Journal, 2, 64-70 (2008).  PDF

 

2007

  • Influence of electric field and mechanical stresses on the fracture of ferroelectrics
    Schneider, G. A.
    Annual Reviews (Materials Research), 37, 491-538, (2007).  Link
  • Finite-element simulation of cantilever vibrations in atomic force acoustic microscopy
    Beltran, F. J. Espinoza; Scholz, T.; Schneider, G. A.; Munoz-Saldana, J.; Rabe, U.; Arnold, W.
    Journal of Physics: Conference Series, 61, 293-297 (2007). Link
  • The dependence of the elastic moduli of reaction bonded alumina on porosity
    Puchegger, S.; Dose, F.; Loidl, D.; Kromp, K.; Janssen, R.; Brandhuber, D.; Hüsing, N.; Peterlik, H.
    Journal of the European Ceramic Society, 27(1), 35-39 (2007). Link
  • Surface modification of Al2O3/TiC cutting ceramics
    Zimmermann, K.; Schneider, G. A.; Bhattacharya, A. K.; Hintze, W.
    Journal of the American Ceramic Society, 90(12), 3773-3778 (2007). Link
  • Measurement of the total energy release rate for cracks in PZT under combined mechanical and electrical loading
    Jelitto, H.; Felten, F.; Swain, M. V.; Balke, H.; Schneider, G. A.
    Journal of Applied Mechanics, 74(6), 1197-1211 (2007). Link
  • Structural Microlayered ceramics with surfaces under tension and compression with increasing apparent fracture  toughness
    Kuebler, J.; Blugan, G.; Jelitto, H.; Schneider, G. A.; Dobedoe, R.
    Key Engineering Materials, 336-338, 2564-2568 (2007). Link
  • Characterization of ferroelectric domains in morphotropic potassium sodium niobate with scanning probe microscopy
    Herber, R.; Schneider, G. A.; Wagner, S.; Hoffmann, M. J.
    Applied Physics Letters, 90, 252905 (2007). Link
  • Surface displacements and surface charges on Ba2CuWO6 and Ba2Cu0.5Zn0.5WO6 ceramics induced by local electric fields investigated with scanning-probe microscopy
    Herber, R.; Schneider, G. A.
    Journal of Materials Research, 22(1), 193-200, (2007). Link
  • Nanoindentation initiated dislocations in barium titanate (BaTiO3)
    Scholz, T.; McLaughlin, K. K.; Giuliani, F.; Clegg, W. J.; Espinoza-Beltran, F. J.; Swain, M. V.; Schneider, G. A.
    Applied Physics Letters, 91, 062903 (2007). Link
  • Fabrication of porous silicon nitride with high porosity 
    Shan, S-Y.; Yang, J.-F.; Gao, J. Q.; Zhang, W. H.; Jin, Z. H.; Janssen, R.; Ohji, T.;
    Key Engineering Materials, Vol. 336-338, 1105-1108 (2007). Link

 

2006 

  • Computational of the stress intensity factor and COD for submicron sized indentation cracks
    Schneider, G. A.; Fett, T.
    Journal of the ceramic Society of Japan,  114, 1044-1048 (2006). Link
  • Characterization of [alpha]-Al2O3-(Al-Si)3Ti composites
    Avraham, S.; Beyer, P.; Janssen, R.; Claussen, N.; Kaplan, W. D.
    Journal of the European Ceramic Society, 26(13), 2719-2726 (2006). Link
  • Thermal stability, structure and mechanical properties of TiSiN coatings prepared by reactive DC magnetron co-sputtering
    García-González, L.; Morales-Hernández, J.; Espinoza-Beltrán, F. J.; Muñoz-Saldaña, J.; Scholz, T.; Schneider, G. A.
    Materials Science Forum, 509, 93-98 (2006). Link
  • Indentation size effect in barium titanate with spherical tipped nanoindenters
    Scholz, T.; Munoz-Saldana, J.; Swain, M. V.; Schneider, G. A.
    Applied Physics Letters, 88(9), 091908-3 (2006). Link

 

2005 

  • Synthesis of fibrous [beta]-Si3N4 structured porous ceramics using carbothermal nitridation of silica
    Yang, J.; Shan, S.; Janssen, R.; Schneider, G.; Ohji, T.; Kanzaki, S.
    Acta Materialia, 53(10), 2981-2990 (2005). Link
  • Zur Bestimmung Bruchmechanischer Kennwerte am Piezo-Aktor
    Häusler, C.; Jelitto, H.; Balke, H.; Schneider, G. A.
    DVM-Bericht 237, 37. Tagung des DVM-Arbeitskreises Bruchvorgänge, S. 355 (2005). PDF
  • Experimenteller Aufbau zur Messung der Energiefreisetzungsrate für Risswachstum in PZT unter Elektromechanischer Last
    Jelitto, H.; Felten, F.; Schneider, G. A.
    DVM-Bericht 237, 37. Tagung des DVM-Arbeitskreises Bruchvorgänge, S. 365 (2005). PDF
  • Processing and characterisation of three-layer alumina-based composites with enhanced damage tolerance
    Arslan, G.; Janssen, R.; Claussen, N.
    Journal of the European Ceramic Society, 25(16), 3553-3561 (2005). Link
  • Cr-Al2O3 layered composites with a high electrical anisotropy prepared by repeated deformation processing
    Leverkoehne, M.; Dakskobler, Ales; Valant, M.; Janssen, R.; Kosmac, Tomaz
    Journal of the European Ceramic Society, 25(1), 65-72 (2005). Link
  • Fracture behavior of poled piezoelectric PZT under mechanical and electrical loads
    Jelitto, H.; Keßler, H.; Schneider, G. A.; Balke, H.
    Journal of the European Ceramic Society, 25(5), 749-757 (2005). Link
  • In situ investigation of subcritical crack growth in lead zirconate titanate ceramics using atomic force microscopy
    Felten, F.; Schneider, G. A.; Knoblauch, V.
    Acta Materialia 53(15), 4051-4056 (2005). Link
  • Measurement of energy release rates for cracks in PZT under electromechanical loads
    Jelitto, H.; Felten, F.; Häusler, C.; Kessler, H.; Balke, H.; Schneider, G. A.
    Journal of the European Ceramic Society, 25(12), 2817-2820 (2005). Link
  • Domain rearrangement during nanoindentation in single-crystalline barium titanate measured by atomic force microscopy and piezoresponse force microscopy
    Schneider, G. A.; Scholz, T.; Munoz-Saldana, J.; Swain, M. V.
    Applied Physics Letters, 86, 192903 (2005). Link
  • On the evolution of the linear material properties of PZT during loading history--an experimental study
    Selten, M.; Schneider, G. A.; Knoblauch, V.; McMeeking, R. M.
    International Journal of Solids and Structures, 42(13), 3953-3966 (2005). Link
  • Porous silicon nitride ceramics prepared by reduction-nitridation of silica
    Shan, S.-Y.; Yang, J.-F.; Gao, J.Q.; Zhang, W.-H.; Jin, Z.H.; Janssen, R.; Ohji, T.; 
    Journal of the American Ceramic Society, 88(9), 2594-2596 (2005). Link
  • Sliding wear of Cr-Al2O3-ZrO2 and Mo-Al2O3-ZrO2 composites 
    Scheppokat, S.; Hannink, R.; Janssen, R.; de Portu, G.; Claussen, N. 
    Journal of the European Ceramic Society, 25(6), 837-845 (2005). Link

 

2004

  • An approximation for electrically semipermeable edge cracks and its application to fracture analysis of PZT
    Kessler, H.; Balke, H.; Jelitto, H.; Schneider, G. A.
    PAMM, 4(1), 282-283 (2004). Link
  • Das instationäre Temperaturfeld bei der reaktiven Infiltration zur Herstellung von Metall-Keramik-Verbundkörpern
    Hussmann, B.; Voges, S.; Eggers, R.; May, M.; Janssen, R.
    Chemie Ingenieur Technik, 76(10), 1534-1538 (2004). Link
  • Calcium phosphate ceramics as substrate for cartilage cultivation
    Janssen, R.; Nagel-Heyer, S.; Goepfert, C.; Pörtner, R.; Toykan, D.; Krummhauer, O.; Morlock, M.; Adamietz, P.; Meenen, N.M.; Kriven, W.M.; Kim, D.K.; Tampieri, A.; Celotti, G.
    Ceramic Engineering and Science Proceedings, 25(4), 523-528 (2004). Link
  • Low cost synthesis of alumina reinforced Fe-Cr-Ni alloys
    Selchert, T.; Janssen, R.; Claussen, N.
    Ceramic Engineering and Science Proceedings, 25(4), 459-464 (2004). Link
  • Processing and wear behavior of Cr-Al2O3-ZrO2 and Mo-Al2O3-ZrO2 composites
    Janssen, R.; Scheppokat, S.; de Portu, G.; Hannink, R.; Claussen, N.
    Ceramic Engineering and Science Proceedings, 25(4), 203-209 (2004). Link
  • Multifunctional metal-ceramic composites by solid free forming
    Janssen, R.; Leverköhne, M.; Coronel, J.J.
    Ceramic Engineering and Science Proceedings, 25(4), 81-88 (2004). Link
  • Cartilage cultivation on a calcium phosphate ceramic in a bioreactor system
    Nagel-Heyer, S.; Janssen, R.; Goepfert, C.; Adamietz, P.; Meenen, N. M.; Pörtner, R.
    Key Engineering Materials, 264-268, 2119-2122 (2004). Link
  • 90° domain configuration and lateral domain wall motion in BaTiO3 evaluated by secondary electron microscopy
    Saldana, J. M.; Moreno, J. M. C.; Schneider, G. A.
    Key Engineering Materials, 264-268, 1185-1188 (2004). Link
  • Modeling and measurement of surface displacements in BaTiO[sub 3] bulk material in piezoresponse force microscopy
    Felten, F.; Schneider, G. A.; Saldana, J. Munoz; Kalinin, S. V.
    Journal of Applied Physics, 96(1), 563-568 (2004). Link
  • Mechanical characterization of thin amorphous tungsten-carbon (W-x C-y) films prepared by DC-cosputtering
    Hurtado Macias, A.; González-Hernández, J.; Muñoz Saldaña, J.; Herrera-Fierro, P.; García-Jiménez, P.; Espinoza Beltrán, F. J.; Scholz, T.; Schneider, G. A.
    Vacuum, 76(2-3), 173-176 (2004). Link
  • Fracture toughness from submicron derived indentation cracks
    Scholz, T.; Schneider, G. A.; Munoz-Saldana, J.; Swain, M. V.
    Applied Physics Letters, 84(16), 3055-3057 (2004).  Link
  • Quasi-static straight and oscillatory crack propagation in ferroelectric ceramics due to moving electric field: experiments and theory
    Niefanger, R.; Pham, V. -B; Schneider, G. A.; Bahr, H. -A; Balke, H.; Bahr, U.
    Acta Materialia, 52(1), 117-127 (2004). Link
  • Invention registration at the TUHH: "Vorrichtung zur Compliance-Messung"
    Inventors: Jelitto, H.; Schneider, G. A.; Felten, F.; Schmidt, K.-D.; Scholz, T.; Swain, M.
    Internal file number TU 045, April 23rd 2004.
  • Processing and properties of sol-gel derived alumina/silicon carbide nanocomposites
    U.N.S. Hareesh, M. Sternitzke, R. Janssen, N. Claussen, K.G. Warrier, "Processing and Properties of Sol-Gel Derived Alumina/Silicon Carbide Nanocomposites", J. Am. 
    Ceram. Soc. 87 [6] (2004) 1024-1030. Link

 

2003 

  • Reaction synthesis of refractory metal-ceramic composites
    Selchert, T.; Janssen, R.; Claussen, N.
    Ceramic Engineering and Science Proceedings, 24(4), 175-180 (2003). Link
  • Pressureless sintering of [beta]-sialon with improved green strength by using metallic Al powder
    Zhang, C.; Janssen, R.; Claussen, N.
    Materials Letters, 57(22-23), 3352-3356 (2003). Link
  • Rapid synthesis of Al2O3 reinforced Fe-Cr-Ni composites
    Travitzky, N.; Kumar, P.; Sandhage, K. H.; Janssen, R.; Claussen, N.
    Materials Science and Engineering A, 344(1-2), 245-252 (2003). Link
  • Mechanical properties and low-temperature aging of tetragonal zirconia polycrystals processed by hot isostatic pressing
    Munoz-Saldana, J.; Balmori-Ramirez, H.; Jaramillo-Vigueras, D.; Iga, T.; Schneider, G. A.
    Journal of Materials Research, 18(10) 2415-2426 (2003). Link
  • Reaktionsgesinterte Mischkeramiken zur Hartbearbeitung
    Hintze, W.; Schneider, G. A.; Püschel, A.
    VDI-Z Spezialwerkzeuge II/2003 September 26-31 (2003). Link
  • Ferroelectric domains in coarse-grained lead zirconate titanate ceramics characterized by scanning force microscopy
    Munoz-Saldana, J.; Hoffmann, M. J.; Schneider, G. A.
    Journal of Materials Research, 18(8), 1777-1786 (2003). Link
  • Nanoindentation measurements on infiltrated alumina-aluminide alloys
    Scholz, T.; May, M.; Swain, M. V.; Schneider, G. A.; Claussen, N.
    International Journal of Materials Research, 94, 819-826 (2003). Link
  • The electrical potential difference across cracks in PZT measured by Kelvin Probe Microscopy and the implications for fracture
    Schneider, G. A.; Felten, F.; McMeeking, R. M.
    Acta Materialia, 51(8), 2235-2241 (2003). Link

 

2002

  • "Fracture mechanical and mechanical properties of piezoelectric ceramics and piezoceramic/electrode interfaces under high electric fields"
    Schneider, G. A.
    in "Piezoelectric Materials in Devices", edited and published by Nava Setter, Ceramics Laboratory, EPFL, Lausanne, Switzerland, p. 195-210 (2002).
  • Reaction bonding and reactive sintering: a way to low cost manufacturing of alumina based components
    Janssen, R.; Claussen, N.; Scheppokat, S.; Roeger, M.
    Materials Integration 4(15), 75-79 (2002).
  • Toughening of alumina/zirconia ceramic composites with silver particles
    Lalande, J.; Scheppokat, S.; Janssen, R.; Claussen, N.
    Journal of the European Ceramic Society, 22(13), 2165-2171 (2002). Link
  • Chapter 5 "Reaction casting of ceramic/metal and ceramic/intermetallic composites"
    Sandhage, K. H.; Claussen, N.
    "Somiya-Handbook: Ceramic Materials and their Applications", 1 (2002).
  • Squeeze Cast beta-Si3N4-Al Composites
    Claussen, N.; Beyer, P.; Janssen, R.; May, M.; Selchert, T.; Yang, J. F.; Ohji, T.; Kanzaki, S.; Yamakawa, A.
    Advanced Engineering Materials, 4(3), 117-119 (2002). Link
  • Electrical resistivity of Cr-Al2O3 and ZrxAly-Al2O3 composites with interpenetrating microstructure
    Leverkoehne, M.; Murthy, V. S. R.; Janssen, R.; Claussen, N.
    Journal of the European Ceramic Society, 22(13), 2149-2153 (2002). Link
  • Phase development of ZrxAly-Al2O3 composites during reaction sintering of Al/ZrO2/Al2O3 powder mixtures
    Leverkoehne, M.; Janssen, R.; Claussen, N.
    Journal of Materials Science Letters, 21(2), 179-183 (2002). Link
  • Preparation of BaTiO3 single crystals using the modified SiO2-exaggerated grain growth method
    Muñoz Saldaña, J.; Mullier, B.; Schneider, G. A.
    Journal of the European Ceramic Society, 22(5), 681-688 (2002). Link
  • High-resolution characterization of piezoelectric ceramics by ultrasonic scanning force microscopy techniques
    Rabe, U.; Kopycinska, M.; Hirsekorn, S.; Saldana, J. Munoz; Schneider, G. A.; Arnold, W.
    Journal of Physics D: Applied Physics, 35(20), 2621-2635 (2002). Link
  • Alumina-Cr and -Nb composites densified by spark plasma sintering
    De la Torre, S. D.; García, D. E.; Claussen, N.; Janssen, R.; Nishikawa, Y.; Miyamoto, H.
    Materials Science Forum by Trans Tech Publications Inc., Vol. 386-388, 299-304 (2002). Link

 

2001 

  • "Fracture of Piezoceramics"
    Schneider, G. A.
    in "Encyclopedia of Materials: Science and Technology", Elsevier, p. 3319-3322 (2001). Link
  • "Reaction Forming"
    Sandhage, K. H.; Claussen, N.
    in "Encyclopedia of Materials: Science and Technology", Elsevier, p. 8035-8040 (2001). Link
  • Reactive casting of metal-ceramic composites
    Claussen, N.; Beyer, P.; Janssen, R.; Kumar, P.; Travitzky, N. A.
    Polish Ceramic Bulletin, 60, 14-20 (2001).
  • Stress induced movement of ferroelastic domain walls in BaTiO3 single crystals evaluated by scanning force microscopy
    Muñoz-Saldaña, J.; Schneider, G. A.; Eng, L. M.
    Surface Science, 480(1-2), L402-L410 (2001). Link
  • Contribution from ferroelastic domain switching detected using X-ray diffraction to R-curves in lead zirconate titanate ceramics
    Glazounov, A. E.; Kungl, H. R. J.; Hoffmann, M. J.; Kolleck, A.; Schneider, G. A.; Wroblewski, T.
    Journal of the American Ceramic Society, 84(12), 2921-2929 (2001). Link
  • Novel in situ-infiltrated Al2O3-metal composites
    Claussen, N.; Schneider, G.A.; Travitzky, N.A.
    Z. Metallk., 92, 7 (2001).
  • Analysis and model of the crack bridging mechanisms in a ductile fiber reinforced ceramic matrix composite
    Hillig, W. B.; Raddatz, O.; Schneider, G. A.; Claussen, N.
    Journal of Materials Science, 36(7), 1653-1663 (2001). Link
  • Mismatched wear couple zirconium oxide and aluminum oxide in total hip arthroplasty
    Morlock, M.; Nassutt, R.; Janssen, R.; Willmann, G.; Honl, M.
    The Journal of Arthroplasty, 16(8), 1071-1074 (2001). Link
  • RBAO: From materials development to commercial components
    Janssen, R.; Claussen, N.; Scheppokat, S.; Röger, M.
    Ceramic Engineering and Science Proceedings, 22(3), 51-58 (2001). Link
  • Reactive casting of ceramic composites (r-3C)
    Kumar, P.; Travitzky, N. A.; Beyer, P.; Sandhage, K. H.; Janssen, R.; Claussen, R.
    Scripta Materialia, 44(5), 751-757 (2001). Link
  • Novel binder system based on paraffin-wax for low-pressure injection moulding of metal-ceramic powder mixtures
    Leverkoehne, M.; Coronel-Hernandez, J.; Dirscherl, R.; Gorlov, I.; Janssen, R.; Claussen, N.